Causes analysis and control measures of coarse grain defects on the surface of hot rolled low-carbon aluminum killed steel strip

LI Xian,YANG Yuebiao,YE Jiang,WEN Baohua,PANG Rui

Steel Rolling ›› 2020, Vol. 37 ›› Issue (5) : 25-29.

Welcome to visit Steel Rolling,
Steel Rolling ›› 2020, Vol. 37 ›› Issue (5) : 25-29. DOI: 10.13228/j.boyuan.issn1003-9996.20190170

Causes analysis and control measures of coarse grain defects on the surface of hot rolled low-carbon aluminum killed steel strip

    {{javascript:window.custom_author_en_index=0;}}
  • {{article.zuoZhe_EN}}
Author information +
History +

HeighLight

{{article.keyPoints_en}}

Abstract

{{article.zhaiyao_en}}

Key words

QR code of this article

Cite this article

Download Citations
{{article.zuoZheEn_L}}. {{article.title_en}}[J]. {{journal.qiKanMingCheng_EN}}, 2020, 37(5): 25-29 https://doi.org/10.13228/j.boyuan.issn1003-9996.20190170

References

References

{{article.reference}}

Funding

RIGHTS & PERMISSIONS

{{article.copyrightStatement_en}}
{{article.copyrightLicense_en}}

Accesses

Citation

Detail

Sections
Recommended

/